Abstract:
The effects of zinc substitution on the nickel based and copper based spinel ferrites
have been investigated. Three series of spinel ferrites with nominal compositions
Ni1-xZnxFe2O4 (x = 0.0, 0.2, 0.4, 0.6, 0.8, 1.0), Cu1-xZnxFe2O4 (x = 0.0, 0.2, 0.4, 0.6, 0.8,
1.0), and Ni0.8-xCuxZn0.2Fe2O4 (x = 0.0, 0.2, 0.4, 0.6, 0.8), were prepared by the
conventional solid state reaction technique. The samples were characterized by SEM, X-
ray diffraction, DC electrical resistivity, dielectric properties and magnetic properties
measurements. Grain size was measured from the scanning electron micrographs. The
average grain size of sintered ferrites was within the range of 2.36-6.16 μm, 26.75-3.25
μm, and 3.15-26.75 μm, for Ni-Zn, Cu-Zn and Ni-Cu-Zn ferrites respectively. The X-rays
diffraction was done through PANalytical diffractometer using Cu Kα radiations (λ =
1.054Å). Lattice constant increased with the increase in zinc concentration in case of Ni1-
xZnxFe2O4
and Cu1-xZnxFe2O4 ferrites, whereas it increased with the increase in copper
concentration in case of Ni0.8-xCuxZn0.2Fe2O4 ferrites. Sintered density increased with the
increase in zinc concentration in case of Ni1-xZnxFe2O4 and Cu1-xZnxFe2O4 ferrites
whereas it increased with the increase in copper concentration in case of
Ni0.8-xCuxZn0.2Fe2O4 ferrites. X-ray density decreased with the increase in zinc
concentration in case of Ni1-xZnxFe2O4 and Cu1-xZnxFe2O4 ferrites whereas it decreased
with the increase in copper concentration in case of Ni0.8-xCuxZn0.2Fe2O4 ferrites. Porosity
decreased with the increase in zinc concentration in case of Ni1-xZnxFe2O4 and Cu1-
xZnxFe2O4
ferrites whereas it decreased with the increase in copper concentration in case
of Ni0.8-xCuxZn0.2Fe2O4 ferrites.
DC electrical resistivity measurements were carried out by two-probe method
from 300 K to 540 K in case of Ni-Zn ferrites, 320 K to 520 K in case of Cu-Zn ferrites
and 305 K to 603 K in case of Ni-Cu-Zn ferrites. Activation energy and drift mobility
were also calculated from the measured resistivity.
The dielectric constant was measured as a function of Zn substitution in Ni-Zn
ferrites as well as a function of Cu concentration in Ni-Cu-Zn ferrites. The dielectric
constant and dielectric loss factors were measured as a function of frequency for all the
samples in the range of 80 Hz to 1 MHz at room temperature. The ac conductivity σac in
case of Ni-Zn ferrites was also measured.
To measure the magnetic properties of the prepared materials, the M-H loop of the
specimen were drawn. From the M-H loop of the sintered materials, we measured
saturation magnetization. Magnetic moment, coercivity and Yafet-Kittel angles were also
calculated.
Saturation magnetization increased up to x = 0.4 and then decreased with the
further increase in Zn concentration in case of Ni-Zn and Cu-Zn ferrites whereas it
decreased with the increase in Cu concentration in case of Ni-Cu-Zn ferrites. The
magnetic moment also had the similar trend. Coercivity decreased with the increase in
Zn concentration in case of Ni-Zn and Cu-Zn ferrites. The Yafet-Kittel (Y-K) angles
initially had zero value and then increased with the rise in Zn concentration for x > 0.2, x
> 0.4, x > 0 in case of Ni-Zn, Cu-Zn and Ni-Cu-Zn ferrites respectively.